Rubber/Graphene Oxide Composites :Interfacial Interaction and Performances  
Rubber/Graphene Oxide Composites :Interfacial Interaction and Performances
资料类型: PDF文件
关键词: Rubber  Graphene  oxide  Interfacial  adhesion  Dielectric  relaxation  
spectra  
资料大小: 100K
所属学科: 分子表征
来源: 第六届亚欧研讨会上处理和性能增强聚合物会议文集(2013.6.2-6 武汉)
简介:
Inpolymercomposites,theinterfacialinteractionbetweenpolymermatrixandfillersisakeyfactorthatgovernsthepropertiesofthefinalcomposites.Inpresentwork,theelastomericcompositesconsistingofgrapheneoxide(GO)sheetsandbutadiene-styrene-vinylpyridinerubber(VPR)werepreparedbyco-coagulationprocesswithdifferentflocculants,hydrogenchlorideandcalciumchloride,inordertoformtwokindsofbondinginterfaces,namelyionicbonding(HVPR)andhydrogenbondinginterfaces(CaVPR).Theinterfacialinteractions(hydrogenbondingandionicinterfacialbonding)werecharacterizedbyXPSandUVspectra.Comparisonoftheeffectsoftheinterfacialinteractiononthepropertiesofthecompositeswasconducted.ItshowedthatthemechanicalpropertiesandgaspermeabilityofHVPR/GOcompositeswereobviouslysuperiortothoseofthecompositeswithhydrogenbondinginterface.Withionicinterfacialbonding,inclusionof3.6vol%ofGOinVPRgenerated21-foldincreaseinglassymodulus,7.5-foldincreaseinrubberymodulus,and3.5-foldincreaseintensilestrength.TheveryfinedispersionofGOandthestrongionicinterfaceinthehybridswereresponsibleforsuchunprecedentedreinforcingefficiencyofGOtowardsVPR.Torevealtheeffectsofinterfacialinteractiononthemoleculardynamics,thedielectricrelaxationspectraofthecompositeshavebeeninvestigated.Resultsshowedthatboththecompositesexhibitedtwodistinctrelaxationprocesses,segmentalrelaxationandinterfacialrelaxation.ConcentrationofGOhadnoimpactonthesegmentaldynamicsofCaVPR,whereas,thesegmentaldynamicsofHVPRsloweddownwhenGOcontentwasabovel.5vol%.Meanwhile,thesegmentalrelaxationofHVPRwasalwaysalittlefasterthanitsCaVPRcounterpart.Inthetemperaturerangeof5一350C,anewrelaxationmode,whichwasslowerthanthesegmentalrelaxationandattributedtotheinterphasewithrestrictedchaindynamics,wasobservedforallthecompositeswithGOloadinglowerthan2.5vol%.TheinterfacialrelaxationtimeofHVPRcontinuouslydecreasedwiththeGOconcentration.However,itdecreasedfirstthenincreasedforCaVPR.Mostinteresting,theinterfacialrelaxationofHVPRwasslowerthanthatforCaVPR.Thee9andthecalculatedfragilityparameterandeffectiveactivationenthalpyoftheinterfacialchainsinHVPRwerealwayshigherthanthoseinCaVPRwiththesameGOconcentration.A11theevidencesindicatedstrongerinterfacialinteractioninHVPRthaninCaVPR.
作者: Z. H. Tang, S. W. Wu, B. C. Guo , L. Q. Zhang
上传时间: 2013-07-01 16:05:21
下载次数: 1
消耗积分: 2  
立即下载:
1人
1人
1人
友情提示:下载后对该资源进行评论,即可奖励2分。
报告错误:  1.下载无效  2. 资料明显无价值  3. 资料重复存在

相关评论 共有0人发表评论 更多评论
你还没有登录,无法发表评论,请首先 登录 注册
免责声明:本站部分资源由网友推荐,来自互联网,版权属于原版权人,如果不慎侵犯到您的权利,敬请告知,我们会在第一时间撤除。本站中各网友的评论只代表其个人观点,不代表本站同意其观点。